Sintered Silicon Carbide (SSIC)
Chemical composition: SiC
Property Value in metric unit Value in US unit
Density 3.1 *10³ kg/m³ 193.5 lb/ft³
Modulus of elasticity 410 GPa 59500 ksi
Flexural strength 450 MPa 65300 psi
Fracture toughness 3.9 MPa*m½ 3.9 MPa*m½
Hardness 25000 HV 25000 HV
Thermal expansion (20 ºC) 4*10-6 ºCˉ¹ 2.2*10-6 in/(in* ºF)
Thermal conductivity 80 W/(m*K) 555 BTU*in/(hr*ft²*ºF)
Max. working temperature 1700 ºC 3090 ºF