Recrystallized Silicon Carbide ceramic (RSC)

(submitted by the website administration)

Recrystallized Silicon Carbide (RSC)
Chemical composition: SiC
Property Value in metric unit Value in US unit
Density 2.7 *10³ kg/m³ 168.5 lb/ft³
Modulus of elasticity 255 GPa 37000 ksi
Flexural strength 100 MPa 14500 psi
Fracture toughness 3 MPa*m½ 3 MPa*m½
Hardness 25000 HV 25000 HV
Thermal expansion (20 ºC) 4.2*10-6 ºCˉ¹ 2.3*10-6 in/(in* ºF)
Thermal conductivity 20 W/(m*K) 139 BTU*in/(hr*ft²*ºF)
Max. working temperature 1650 ºC 3000 ºF