Nitride Bonded Silicon Carbide (NSC)
Chemical composition: SiC
Property Value in metric unit Value in US unit
Density 2.82*10³ kg/m³ 176 lb/ft³
Modulus of elasticity 195 GPa 28300 ksi
Flexural strength 200 MPa 29000 psi
Thermal expansion (20 ºC) 4.2*10-6 ºCˉ¹ 2.3*10-6 in/(in* ºF)
Thermal conductivity 14.5 W/(m*K) 101 BTU*in/(hr*ft²*ºF)
Max. working temperature 1450 ºC 2640 ºF