| Elastomer | ||||
| Silicone | ||||
| Property | Value in metric unit | Value in US unit | ||
| Density | 0.98 *10³ | kg/m³ | 61.2 | lb/ft³ | 
|---|---|---|---|---|
| Tensile strength | 10 | MPa | 1450 | psi | 
| Elongation | 700 | % | 700 | % | 
| Glass transition temperature | -50 | ºC | -58 | ºF | 
| Maximum work temperature | 300 | ºC | 572 | ºF | 
| Electric resistivity | 103 -109 | Ohm*m | 105 -1011 | Ohm*cm | 
| Dielectric constant | 3.3 | - | 3.3 | - | 
Applications: high temperature sealant, adhesives, vibration damping components.