Property Value in metric unit Value in US unit
Density 1.23 *10³ kg/m³ 76.8 lb/ft³
Tensile strength 25 MPa 3630 psi
Elongation 1000 % 1000 %
Glass transition temperature -50 ºC -58 ºF
Maximum work temperature 100 ºC 212 ºF
Electric resistivity 103 Ohm*m 105 Ohm*cm
Dielectric constant 9 - 9 -
  • Excellent abrasion resistance;
  • Good resistance to oil, fuel and petroleum based solvents;
  • Excellent resistance to ozone;
  • Very good resistance to sunlight;
  • Poor resistance to lacquer solvents.

Applications: oil and crude oil hoses, gaskets, diaphragms, lining of chemical vessels.

Related internal links

Related external links

elastomer_neoprene_chloroprene.txt · Last modified: 2012/06/03 by dmitri_kopeliovich
Promote in SubsTech       Creative Commons License Except where otherwise noted, this work is licensed under a Creative Commons Attribution-Noncommercial-Share Alike 3.0 License