AISI 430
Chemical composition: C=0.12%max, Mn=1%max, Cr=17%
Property Value in metric unit Value in US unit
Density 7.8 *10³ kg/m³ 487 lb/ft³
Modulus of elasticity 200 GPa 29000 ksi
Thermal expansion (20 ºC) 10.4*10-6 ºCˉ¹ 5.78*10-6 in/(in* ºF)
Specific heat capacity 460 J/(kg*K) 0.11 BTU/(lb*ºF)
Thermal conductivity 26.1 W/(m*K) 181 BTU*in/(hr*ft²*ºF)
Electric resistivity 6.0*10-7 Ohm*m 6.0*10-5 Ohm*cm
Tensile strength (annealed) 517 MPa 75000 psi
Yield strength (annealed) 310 MPa 45000 psi
Elongation (annealed) 32 % 32 %
Hardness (annealed) 82 RB 82 RB
Tensile strength (cold drawn) 586 MPa 85000 psi
Yield strength (cold drawn) 483 MPa 70100 psi
Elongation (cold drawn) 20 % 20 %
Hardness (cold drawn) 90 RB 90 RB

Related internal links

Related external links

stainless_steel_aisi_430.txt · Last modified: 2012/06/02 by dmitri_kopeliovich
Promote in SubsTech       Creative Commons License Except where otherwise noted, this work is licensed under a Creative Commons Attribution-Noncommercial-Share Alike 3.0 License