Chemical composition: MgO
Property Value in metric unit Value in US unit
Density 3.4 *10³ kg/m³ 212.2 lb/ft³
Modulus of elasticity 250 GPa 36300 ksi
Flexural strength 165 MPa 23900 psi
Thermal expansion (20 ºC) 13.5*10-6 ºCˉ¹ 7.5*10-6 in/(in* ºF)
Thermal conductivity 9 W/(m*K) 62.4 BTU*in/(hr*ft²*ºF)
Specific heat capacity 880 J/(kg*K) 0.21 BTU/(lb*ºF)
Dielectric constant (1MHz) 10 - 10 -