Magnesia ceramic (30% porosity)

(submitted by the website administration)

Magnesia ceramic (30% porosity)
Chemical composition: MgO
Property Value in metric unit Value in US unit
Density 2.5 *10³ kg/m³ 156.1 lb/ft³
Modulus of elasticity 90 GPa 13050 ksi
Flexural strength 50 MPa 7250 psi
Thermal expansion (20 ºC) 12*10-6 ºCˉ¹ 6.7*10-6 in/(in* ºF)
Thermal conductivity 8 W/(m*K) 55.5 BTU*in/(hr*ft²*ºF)
Specific heat capacity 880 J/(kg*K) 0.21 BTU/(lb*ºF)
Dielectric constant (1MHz) 10 - 10 -