Aluminum Titanate Ceramic ATI
Chemical composition: Al2TiO5
Property Value in metric unit Value in US unit
Density 3.4 *10³ kg/m³ 212.2 lb/ft³
Modulus of elasticity 30 GPa 4350 ksi
Flexural strength 60 MPa 8700 psi
Fracture toughness 4 MPa*m½ 4 MPa*m½
Thermal expansion (20 ºC) 1*10-6 ºCˉ¹ 0.6*10-6 in/(in* ºF)
Thermal conductivity 2 W/(m*K) 13.9 BTU*in/(hr*ft²*ºF)
Specific heat capacity 800 J/(kg*K) 0.19 BTU/(lb*ºF)
Max. working temperature 1100 ºC 2010 ºF