Property Value in metric unit Value in US unit
Viscosity (mixed) at 77°F (25°C) 12000 cP 0.251 lbf*sec/ft²
Working strength time 5 min 5 min
Full cure time 24 hrs 24 hrs
Maximum gap 2 mm 0.08 in
Shear strength, steel-to-steel 77°F (25°C) 13 MPa 1885 psi
Peel strength, steel-to-steel 77°F (25°C) 45 N/(25mm width) 10 PIW (lbf/inch width)
Min. service temperature -40 ºC -40 ºF
Max. service temperature 80 ºC 175 ºF