Silicate ceramic Steatite C221 | ||||
Chemical composition: SiO2, MgO, Al2O3 | ||||
Property | Value in metric unit | Value in US unit | ||
Density | 2.7 *10³ | kg/m³ | 168.5 | lb/ft³ |
---|---|---|---|---|
Modulus of elasticity | 110 | GPa | 15950 | ksi |
Flexural strength | 140 | MPa | 20300 | psi |
Compressive strength | 900 | MPa | 130500 | psi |
Thermal expansion (20 ºC) | 7.0*10-6 | ºCˉ¹ | 3.9*10-6 | in/(in* ºF) |
Thermal conductivity | 2.5 | W/(m*K) | 17.3 | BTU*in/(hr*ft²*ºF) |
Dielectric constant | 6 | - | 6 | - |
http://www.me.unm.edu/~zleseman/Lecture5.pdf
http://www.virginia.edu/bohr/mse209/home.htm
http://www.scs.uiuc.edu/~chem584/lectures/chem584.ceramics.pdf
http://bioe.eng.utoledo.edu/adms_staffs/akkus/BIO2200_notes/Ceramics.ppt
http://www.egr.msu.edu/classes/me477/hinds/Powerpoint/Ch07-Ceramics-Wiley.ppt
http://info.lu.farmingdale.edu/depts/met/met205/ceramics/ceramics.PPT
http://www.mse.eng.ohio-state.edu/~flores/mse205/Chapter_19_pres.pdf
http://me.queensu.ca/courses/mech412/Notes/Lecture06.ppt
http://www.ims.uconn.edu/~bhuey/MMAT244/4.pdf
http://bioe.eng.utoledo.edu/adms_staffs/akkus/BIO2200_notes/Ceramics.ppt