Polyether Ether Ketone B Matrix Composite reinforced by 30% carbon fibers

(submitted by the website administration)

Carbon Fiber Reinforced Polymer (CFRP)
Composition: 30% carbon fibers in polyether ether ketone B (PEEK) matrix
Property Value in metric unit Value in US unit
Density 1.4 *10³ kg/m³ 88 lb/ft³
Tensile modulus 22.3 GPa 3200 ksi
Tensile strength 215 MPa 31000 psi
Elongation at break 1.8 % 1.8 %
Flexural strength 298 MPa 43000 psi
Thermal expansion (20 ºC) 15*10-6 ºCˉ¹ 8.3*10-6 in/(in* ºF)