Composition: carbon matrix + carbon fibers
Property Value in metric unit Value in US unit
Modulus of elasticity 135 GPa 19600 psi
Tensile strength 650 MPa 94300 psi
Compressive strength 650 MPa 94300 psi
Fracture energy 1.7 kJ/m2 0.15 BTU/ft2