Sawing fluid
Semi-synthetic fluid
Property Value in metric unit Value in US unit
Density at 60°F (15.6°C) 1.02 *10³ kg/m³ 63.7 lb/ft³
Flash point 166 ºC 330 ºF
PH, 5% emulsion 9.2 9.2


Used as emulsion in soft water at concentrations 5-10%.
Applications:sawing of steels and cast irons.