| Industrial gear oil ISO 68 | ||||
| Mineral based gear oil | ||||
| Property | Value in metric unit | Value in US unit | ||
| Density at 60°F (15.6°C) | 0.878 *10³ | kg/m³ | 54.8 | lb/ft³ | 
|---|---|---|---|---|
| Kinematic viscosity at 104°F (40°C) | 67.5 | cSt | 67.5 | cSt | 
| Kinematic viscosity at 212°F (100°C) | 8.6 | cSt | 8.6 | cSt | 
| Viscosity index | 97 | 97 | ||
| Timken OK load | 27.5 | kg | 60.6 | lb. | 
| Flash point | 242 | ºC | 468 | ºF | 
| Pour Point | -30 | ºC | -22 | ºF | 
| AGMA No. | 2EP | 2EP | ||
| Color | 1.0 | 1.0 | ||