Sintered aluminum alloy A

(submitted by the website administration)

Sintered aluminum alloy A
Chemical composition: Si=0.6%, Cu=0.25%, Mg=1%, Al+Al2O3 balance
Property Value in metric unit Value in US unit
Density 90% of theoretical density
Modulus of elasticity 61 GPa 8800 ksi
Thermal conductivity 160 W/(m*K) 1110 BTU*in/(hr*ft²*ºF)
Electric resistivity 4.5*10-8 Ohm*m 4.5*10-6 Ohm*cm
Tensile strength (T1) 139 MPa 20100 psi
Yield strength (T1) 88 MPa 12700 psi
Elongation (T1) 5 % 5 %
Tensile strength (T4) 172 MPa 24900 psi
Yield strength (T4) 114 MPa 16600 psi
Elongation (T4) 5 % 5 %
Shear strength (T4) 131 MPa 19000 psi
Compressive strength (T4) 174 MPa 25300 psi
Tensile strength (T6) 232 MPa 33600 psi
Yield strength (T6) 224 MPa 32500 psi
Elongation (T6) 2 % 2 %
Shear strength (T6) 139 MPa 20100 psi
Compressive strength (T6) 175 MPa 25400 psi

Related internal links

Related external links

sintered_aluminum_alloy_a.txt · Last modified: 2012/06/02 by dmitri_kopeliovich
Promote in SubsTech       Creative Commons License Except where otherwise noted, this work is licensed under a Creative Commons Attribution-Noncommercial-Share Alike 3.0 License