Typical SiC Matrix Composite reinforced by SiC long fibers

(submitted by the website administration)

Typical SiC matrix reinforced by SiC long fibers
Composition: Silicon carbon (SiC) matrix + SiC long (cont.) fibers
Property Value in metric unit Value in US unit
Density 2.1 *10³ kg/m³ 131 lb/ft³
Modulus of elasticity 96 GPa 13900 ksi
Tensile strength 262 MPa 38000 psi
Compressive strength 450 MPa 65260 psi
Shear strength 34 MPa 4930 psi
Thermal expansion (20 ºC) 2.7*10-6 ºCˉ¹ 1.5*10-6 in/(in* ºF)
Thermal conductivity 1.32 W/(m*K) 9.2 BTU*in/(hr*ft²*ºF)