Typical alumina matrix SiC reinforced by long fibers
Composition: alumina (Al2O3) matrix + SiC long (continuous) fibers
Property Value in metric unit Value in US unit
Density 2.82 *10³ kg/m³ 176 lb/ft³
Modulus of elasticity 124 GPa 18000 ksi
Tensile strength 365 MPa 53000 psi
Compressive strength 270 MPa 39200 psi
Shear strength 15.2 MPa 2200 psi
Thermal expansion (20 ºC) 8.5*10-6 ºCˉ¹ 4.7*10-6 in/(in* ºF)