Synthetic cutting fluid concentrate

(submitted by the website administration)

Synthetic cutting fluid concentrate
Synthetic fluid
Property Value in metric unit Value in US unit
Density at 60°F (15.6°C) 1.085 *10³ kg/m³ 67.7 lb/ft³
PH 9.8 9.8
Acid value 44 meqKOH/g 44 meqKOH/g


Used in water diluted condition at concentrations 4-7%. Applications: grinding,sawing, drilling, tapping, milling, turning.