Composition: Silicon carbon (SiC) matrix + SiC long (cont.) fibers (13 mkm diameter)
Property Value in metric unit Value in US unit
Density 2.74 *10³ kg/m³ 171 lb/ft³
Modulus of elasticity 270 GPa 39160 ksi
Tensile strength 217 MPa 31500 psi
Thermal expansion (20 ºC) 3.5*10-6 ºCˉ¹ 1.9*10-6 in/(in* ºF)
Thermal heat capacity 630 J/(kg*K) 0.15 BTU/(lb*ºF)
Thermal conductivity 4 W/(m*K) 27.7 BTU*in/(hr*ft²*ºF)