SiC Matrix Composite reinforced by SiC long fibers (Dow Sylramic)

(submitted by the website administration)

Dow Sylramic
Composition: Silicon carbon (SiC) matrix + SiC long (cont.) fibers (10 mkm diameter)
Property Value in metric unit Value in US unit
Density 3.05 *10³ kg/m³ 190 lb/ft³
Modulus of elasticity 395 GPa 57300 ksi
Thermal expansion (20 ºC) 5.4*10-6 ºCˉ¹ 3.0*10-6 in/(in* ºF)
Thermal heat capacity 630 J/(kg*K) 0.15 BTU/(lb*ºF)
Thermal conductivity 42 W/(m*K) 291 BTU*in/(hr*ft²*ºF)