| Hydraulic oil ISO 150 | ||||
| Mineral based hydraulic oil | ||||
| Property | Value in metric unit | Value in US unit | ||
| Density at 60°F (15.6°C) | 0.882 *10³ | kg/m³ | 55.1 | lb/ft³ |
|---|---|---|---|---|
| Kinematic viscosity at 104°F (40°C) | 147 | cSt | 147 | cSt |
| Kinematic viscosity at 212°F (100°C) | 14.6 | cSt | 14.6 | cSt |
| Viscosity index | 98 | 98 | ||
| Flash point | 286 | ºC | 547 | ºF |
| Pour Point | -24 | ºC | -11 | ºF |
| Aniline Point | 119 | ºC | 246 | ºF |
| Color | max. 3.5 | max. 3.5 | ||