to Cast aluminum alloys
to Properties of aluminum alloys

Cast aluminum alloy 443.0

(submitted by the website administration)

Cast aluminum alloy 443.0
Chemical composition: Si=5.3%, Al balance, permanent mold casting
Property Value in metric unit Value in US unit
Density 2.69 *10³ kg/m³ 168 lb/ft³
Modulus of elasticity 71 GPa 10300 ksi
Thermal expansion (20 ºC) 22.1*10-6 ºCˉ¹ 12.3*10-6 in/(in* ºF)
Specific heat capacity 963 J/(kg*K) 0.230 BTU/(lb*ºF)
Thermal conductivity 146 W/(m*K) 1010 BTU*in/(hr*ft²*ºF)
Electric resistivity 4.6*10-8 Ohm*m 4.6*10-6 Ohm*cm
Heat of fusion 3.89*105 J/kg 167 BTU/lb
Liquidus temperature 632 ºC 1170 ºF
Solidus temperature 574 ºC 1065 ºF
Tensile strength (F) 160 MPa 23200 psi
Yield strength (F) 70 MPa 10150 psi
Elongation (F) 6 % 6 %
Shear strength (F) 91 MPa 13200 psi
Hardness (F) , range 30-60 HB 30-60 HB

Related internal links

Related external links

http://www.tntech.edu/me/courses/Zhang/ME30103110/Chap11pt4.ppt
http://www.ccm.udel.edu/Personnel/homepage/class_web/Lecture%20Notes/2004/AskelandPhuleNotes- CH13Printable.ppt
http://www.aluminum.org/
http://www.aluminium.org/
http://www.cmse.ed.ac.uk/MSE3/Topics/MSE3-nonferrous.pdf
http://www.ndt-ed.org/GeneralResources/MaterialProperties/ET/et_matlprop_index.htm

to Cast aluminum alloys
to Properties of aluminum alloys