Alumina Matrix Composite reinforced by SiC whiskers

(submitted by the website administration)

Alumina matrix reinforced by SiC whiskers
Composition: alumina (Al2O3 matrix + 25% SiC whiskers
Property Value in metric unit Value in US unit
Density 3.7 *10³ kg/m³ 231 lb/ft³
Modulus of elasticity 390 GPa 56560 ksi
Flexural strength 900 MPa 130500 psi
Fracture toughness 8.0 MPa*m½ 8.0 MPa*m½
Thermal expansion (20 ºC) 6*10-6 ºCˉ¹ 3.3*10-6 in/(in* ºF)